GAS METAL ARC WELDING - Practice Mode

1) Which type of defect is caused if the gas flowing rate is uneven?
Correct Answer: Porosity
2) What is the difficulty in starting of arc in GMAW?
Correct Answer: Wrong polarity
3) How to troubleshoot the burn back problem if the contact tip is plugged or worn out?
Correct Answer: Clean and replace contact tip
4) What do you call a weld joint having small holes/cavities due to entrapped gas packets?
Correct Answer: Porosity
5) What is the defect in a weld joint, in which the weld metal melting through base metal resulting in holes?
Correct Answer: Burn through